Anti corrosion pool project

 Details
Thickness1.0mm 2.0mm 3.0mm
Surface FinishSelf-leveling trowel finish, roller finish, glossy finish
Service LifeOver 10 years
Floor CharacteristicsReinforced with glass fiber for improved tensile strength; non-toxic, odorless, and excellent in resistance to acid, alkali and chemical solvents.
Scope of Application① General chemical storage tanks;
② Crack-resistant flooring, pharmaceutical factories, power plants, non-ferrous metal factories;
③ Premises with special anti-corrosion requirements.
Construction Process
①Waterproofing TreatmentWaterproofing construction shall be completed for ground floors.
②Base TreatmentGrind, repair and remove dust according to the condition of the substrate.
③Epoxy PrimerApply 1 to 2 roller coats of epoxy primer with high permeability and adhesion to enhance substrate strength and bonding force.
④Anti-corrosion Epoxy PrimerApply one roller coat of sealing anti-corrosion epoxy primer with strong adhesion to improve bonding between the base surface and glass fiber cloth.
⑤Glass Fiber Cloth LayingLay the glass fiber cloth flat, adhere it to the floor with mixed epoxy intermediate coating, then level evenly with a trowel to ensure uniform coverage and improve floor toughness. Apply 1 to 3 layers as required.
⑥Anti-corrosion Epoxy Intermediate CoatMix epoxy intermediate coating with appropriate quartz sand, and apply evenly 1 to 3 coats with a trowel.
⑦Anti-corrosion Epoxy PuttyApply 2 to 3 coats as required until the surface is flat and pore-free, suitable for subsequent topcoat application.
⑧Anti-corrosion Epoxy Color CoatApply two roller coats of anti-corrosion epoxy color paint for uniform color appearance.
⑨Anti-corrosion Epoxy TopcoatTrowel one coat of anti-corrosion epoxy self-leveling topcoat, or apply two roller coats of anti-corrosion clear coat. The finished floor is bright, clean and uniform in color.
⑩Completion & CuringPedestrian access permitted after 24 hours; heavy load access after 72 hours; put into official use after 7 days of curing. (Based on 25℃; opening time shall be properly extended at low temperature. Keep the floor free of water during curing.)
Technical Specifications
ItemIndex
Surface Drying Time (h)≤4
Hard Drying Time (h)≤24
Hardness (Shore D)≥80
Wear Resistance (750g/500r, weight loss, g)≤0.03
Compressive Strength (MPa)≥80
Tensile Strength (MPa)≥100
Bonding Strength (MPa)≥3
Note: Refer to Appendix 2 for anti-corrosion performance.
Process Diagram
691a89b0136c6.jpg


Contact Us—— Business covers major, medium and small cities across China as well as Southeast Asian countries.
Guangdong Jinfeng New Material Technology Co., Ltd.
Address: Room 1909, Building 5, Huixing Commercial Building, Shilong Town, Dongguan City, Guangdong ProvinceContact Person: Ms. Wang 15015150026Website: /Email:1841896008@qq.com
Taiwan Branch Office
Address:6th Floor, No. 23, Lane 17, Section 1, Touzhang Road, Toujia Village, Tanzi Township, Taichung City, Taiwan
Tel:00886-4-25326538
Fax:00886-4-25326538
Headquarters Production Base
Address: Zhuli Industrial Zone, Shiwan Town, Huizhou City, Guangdong Province (Jinfeng Company)
Tel: Ms. Wang 15015150026
  • Jinfeng Tiktok
  • WeChat Channels
Consulting service

Phone

Business Inquiry

15015150026

Douyin account

Douyin account

Video Channel

Video Channel

Top

Consulting service